Nylon types: PA6, PA12, and CF-nylon

"Nylon" covers several different materials. Here is how the common filament types compare.

The short answer

PA6 is often chosen for toughness and wear resistance. PA12 is often chosen because it tends to be easier to print and more dimensionally stable. Carbon-fiber nylon adds stiffness and a matte finish, but needs a hardened nozzle.

Side-by-side

PA6 (and PA6 blends)PA12CF-nylon (PA-CF)
Known forToughness and wear resistanceSteadier dimensions, some flexibilityStiffness and a matte finish
Moisture sensitivityHighGenerally lower than PA6Depends on the base nylon
WarpingCan warp noticeablyOften warps less than PA6Carbon fibers often reduce shrinkage-related warping compared with similar unfilled nylons
Typical nozzle rangeAbout 250–290 °CAbout 240–270 °CAbout 250–300 °C
NozzleBrass is commonly used for unfilled nylonsBrass is commonly used for unfilled nylonsHardened nozzle strongly recommended
EnclosureStrongly recommendedRecommendedStrongly recommended

These ranges are general guidance only. Nylon blends vary a lot between brands, so start with your filament maker's recommended settings and adjust from there, staying within the limits of your printer and hotend.

PA6

PA6 is a widely used engineering nylon. It is valued for toughness and wear resistance, which makes it a frequent pick for gears, bushings, and hard-working clips. It tends to absorb moisture readily and can warp, so drying and an enclosure matter. Some filaments are PA6/66 copolymers or other blends; follow that product's settings.

PA12

PA12 generally absorbs less moisture and is often easier to print than many PA6 formulations. It can be a good first nylon. It still benefits from dry storage.

Carbon-fiber nylon (PA-CF)

Short chopped carbon fibers are added to a nylon base (often PA6 or PA12). This usually makes parts stiffer and gives a matte finish, and many makers find it warps less than unfilled nylon. The fibers are abrasive, so a hardened steel or similar wear-resistant nozzle is strongly recommended. Parts are usually stiffer but may be less flexible than unfilled nylon.

Other nylons you may see