Fixing warping and moisture problems

Many nylon printing problems come from moisture or uneven cooling. Work through these checks in order.

Corners lifting off the bed

  1. Clean the bed according to the bed maker's instructions.
  2. Check the first layer. It should be lightly pressed down, not round and loose. Re-level or adjust Z offset if needed.
  3. Use a suitable surface such as garolite, or PEI with glue stick or a nylon-specific adhesive.
  4. Add a brim or corner "mouse ears."
  5. Raise the bed temperature slightly while staying within the limits recommended by your printer and filament manufacturer.
  6. Close the enclosure and preheat it before printing.

Layers splitting or cracking

  1. Stop drafts by closing the enclosure and keeping the printer away from fans and vents.
  2. Reduce part cooling.
  3. Raise the nozzle temperature in small steps within the maker's recommended range.
  4. Dry the filament. Moisture can weaken layer bonding.

Bubbles, popping, or rough surfaces

These are common signs that the filament has absorbed moisture. Dry the spool following the maker's guidance, then print from a sealed dry box. See drying and storing nylon.

Stringing

Under-extrusion or clogs with CF-nylon

Design changes that help

Back to the nylon printing guide.